Mechanical Properties (TYPICAL) |
|
---|---|
Yield Strength | 160 Ksi (TYPICAL) |
Tensile Strength | 170-190 Ksi (TYPICAL) |
Elongation in 2″, % (min) | 15% In 2″ (TYPICAL) |
AR 400- Chemical Composition
Chemistry (%) | |
---|---|
CARBON | Max C 17 |
MANGANESE | Max Mn 1.50 |
PHOSPHORUS | Max P .015 |
SULPHER | Max S .005 |
SILICONE | Max Si .60 |
MOLYBDENUM | Max Mo .40 |
BORON | Min B .0005 |
CE (TYPICAL) | .42 < 1/2″ .48 > 1/2″ |
AR 400 – Forming Properties90 Degree Bend All Gauges
Bend Axis | Transverse to Rolling Direction | Longtudinal to Rolling Direction |
---|---|---|
(Easy Way) | (Hard Way) | |
R/T – Punch Radius / Thickness | 3 | 4 |